Initiation of Stress Corrosion Cracks in X80 and X100 Pipe Steels in Near-Neutral pH Environment

Tests were conducted on X80 and X100 pipe steels at 95% specified minimum yield stress in NS4 solution mixed with soil using specimens machined along the transverse direction of the pipes. Crack initiation in X100 is much easier than in X80. With test time increasing from 110 to 220 days, less numer... Full description

Contained in: Journal of Materials Engineering and Performance Vol. 25, No. 1 (2016), p. 227-240
Fulltext access:
Availability is being checked...
Interlibrary loan: Check possibility for interlibrary loan
Links: Additional Link (dx.doi.org)
Additional Keywords: FLIESSSPANNUNG
NEUTRALER-PH-WERT
NEUTRALES-PH-MILIEU
QUERRICHTUNG
RISSAUSBREITUNG
RISSSPITZE
ROHRSTAHL
SCHICHTDICKE
SPANNUNGSKORROSION
SPANNUNGSRISSKORROSION
WACHSTUMSGESCHWINDIGKEIT
DOI: 10.1007/s11665-015-1822-5
Notes: Copyright: Metadaten: TEMA, Copyright WTI-Frankfurt eG
Copyright: (C) Alle Rechte beim Herausgeber
Physical Description: 14 Seiten
ID (e.g. DOI, URN): 10.1007/s11665-015-1822-5
PPN (Catalogue-ID): WTI000391220
Note: WTI TEMA DB
more publication details ...

Associated Publications/Volumes

  • Associated records are being queried...
more (+)
Internes Format
LEADER 02210nma a2200433 c 4500
001 WTI000391220
003 DE-601
005 20190329003208.0
007 cr uuu---uuuuu
008 171221s2016 000 0 und d
024 7 |a 10.1007/s11665-015-1822-5  |2 doi 
028 5 2 |a TEMA1607_wti_pica 
035 |a (DE-599)WTI20160113115 
040 |b ger  |c GBVCP 
084 |a A  |2 FIZTtc 
084 |a 3KEB  |a 3KXU  |a 3KXM  |2 FON2006 
245 0 0 |a Initiation of Stress Corrosion Cracks in X80 and X100 Pipe Steels in Near-Neutral pH Environment  |h Elektronische Ressource 
300 |a Online-Ressource  |a 14 Seiten 
500 |a Copyright: Metadaten: TEMA, Copyright WTI-Frankfurt eG 
500 |a Copyright: (C) Alle Rechte beim Herausgeber 
520 |a Tests were conducted on X80 and X100 pipe steels at 95% specified minimum yield stress in NS4 solution mixed with soil using specimens machined along the transverse direction of the pipes. Crack initiation in X100 is much easier than in X80. With test time increasing from 110 to 220 days, less numerous but deeper cracks were found in both pipe steels. Cracks showed higher growth rates in the transverse specimens than those in longitudinal ones. TEM results revealed concentration of Ni or Cr elements, formation of oxide layer at crack walls, and TiN-related dissolution at the crack tip. 
653 4 |a RISSAUSBREITUNG 
653 4 |a SPANNUNGSRISSKORROSION 
653 4 |a SPANNUNGSKORROSION 
653 4 |a ROHRSTAHL 
653 4 |a NEUTRALES-PH-MILIEU 
653 4 |a SCHICHTDICKE 
653 4 |a WACHSTUMSGESCHWINDIGKEIT 
653 4 |a RISSSPITZE 
653 4 |a FLIESSSPANNUNG 
653 4 |a QUERRICHTUNG 
653 4 |a NEUTRALER-PH-WERT 
773 0 8 |i In  |t Journal of Materials Engineering and Performance  |g Vol. 25, No. 1 (2016), p. 227-240  |q 25:1<227-240 
856 4 0 |u http://dx.doi.org/10.1007/s11665-015-1822-5 
912 |a GBV_WTI 
950 |a Rissausbreitung  |a Spannungsrisskorrosion  |a Spannungskorrosion  |a Rissinitiierung  |a Rohrstahl  |a neutrales pH-Milieu  |a Schichtdicke  |a Wachstumsrate  |a Rissspitze  |a Fließspannung  |a Querrichtung  |a neutraler pH-Wert  |2 DE-601 
950 |a Risswachstumsgeschwindigkeit  |2 DE-601 
951 |a AR 
952 |d 25  |j 2016  |e 1  |h 227-240