Boric acid free nickel electrolyte for plating of electrical contacts

Prior to plating of electrical contacts with noble metals such as palladium or gold often an intermediate layer of nickel is applied. Owing to reasons of occupational safety and environmental protection a boric acid free nickel electrolyte for 'High-Speed'-applications has been developed by HARTING.... Full description

Main Author: Riechmann, H.
Contributors: MÜơller, M. | Author
Meyerovich, A. | Author
Contained in: Transactions of the Institute of Metal Finishing. The International Journal for Surface Engineering and Coatings Vol. 95, No. 2 (2017), p. 73-77
Fulltext access:
Availability is being checked...
Interlibrary loan: Check possibility for interlibrary loan
Links: Additional Link (dx.doi.org)
ISSN: 0020-2967
1745-9192
Additional Keywords: ABRIEBFESTIGKEIT
ARBEITSSCHUTZ
BORSAEURE
EIGENSPANNUNG
ELEKTRISCHER-KONTAKT
ELEKTROLYT
GOLD
KONTAMINATION
KORROSIONSBESTAENDIGKEIT
KORROSIONSSCHUTZ
PALLADIUM
PLATTIEREN
SCHMUTZSTOFF
UMWELTSCHUTZ
VERNICKELN
ZWISCHENSCHICHT
DOI: 10.1080/00202967.2016.1268841
Language: English
Notes: Copyright: Metadaten: TEMA, Copyright WTI-Frankfurt eG
Copyright: (C) Alle Rechte beim Herausgeber
Physical Description: 5 Seiten, 13 Quellen
ID (e.g. DOI, URN): 10.1080/00202967.2016.1268841
PPN (Catalogue-ID): WTI004264673
Note: WTI TEMA DB
more publication details ...

Associated Publications/Volumes

  • Associated records are being queried...
more (+)
Internes Format
LEADER 02813nma a2200517 c 4500
001 WTI004264673
003 DE-601
005 20171222020233.0
007 cr uuu---uuuuu
008 171222s2017 000 0 eng d
024 7 |a 10.1080/00202967.2016.1268841  |2 doi 
035 |a (DE-599)WTI20170400128 
040 |b ger  |c GBVCP 
041 0 |a eng 
084 |a A  |2 FIZTtc 
084 |a 3KU  |a 3BXP  |a 3KXU  |a 3MD  |2 FON2006 
100 1 |a Riechmann, H.  |e verfasserin  |4 aut 
245 1 0 |a Boric acid free nickel electrolyte for plating of electrical contacts  |h Elektronische Ressource 
300 |a Online-Ressource  |a 5 Seiten, 13 Quellen 
500 |a Copyright: Metadaten: TEMA, Copyright WTI-Frankfurt eG 
500 |a Copyright: (C) Alle Rechte beim Herausgeber 
520 |a Prior to plating of electrical contacts with noble metals such as palladium or gold often an intermediate layer of nickel is applied. Owing to reasons of occupational safety and environmental protection a boric acid free nickel electrolyte for 'High-Speed'-applications has been developed by HARTING. It was shown by examination in laboratory and pilot plant scale that the newly developed electrolyte generates layers of equal quality to layers generated with a conventional boric acid buffered Watts electrolyte. Single characteristics of the layer generated with the new electrolyte that are in particular important for connectors, e.g. corrosion and abrasion resistance, residual stress, compatibility with contaminants and buffer stability, are very good compared to those of the layers generated with the conventional Watts electrolyte. 
653 4 |a ELEKTRISCHER-KONTAKT 
653 4 |a PLATTIEREN 
653 4 |a BORSAEURE 
653 4 |a ELEKTROLYT 
653 4 |a KORROSIONSSCHUTZ 
653 4 |a ABRIEBFESTIGKEIT 
653 4 |a ZWISCHENSCHICHT 
653 4 |a VERNICKELN 
653 4 |a PALLADIUM 
653 4 |a GOLD 
653 4 |a KONTAMINATION 
653 4 |a SCHMUTZSTOFF 
653 4 |a ARBEITSSCHUTZ 
653 4 |a KORROSIONSBESTAENDIGKEIT 
653 4 |a EIGENSPANNUNG 
653 4 |a UMWELTSCHUTZ 
700 1 |a MÜơller, M.  |e verfasserin  |4 aut 
700 1 |a Meyerovich, A.  |e verfasserin  |4 aut 
773 0 8 |i In  |t Transactions of the Institute of Metal Finishing. The International Journal for Surface Engineering and Coatings  |g Vol. 95, No. 2 (2017), p. 73-77  |q 95:2<73-77  |x 0020-2967  |x 1745-9192  |x 0020-2967 
856 4 0 |u http://dx.doi.org/10.1080/00202967.2016.1268841 
912 |a GBV_WTI 
950 |a elektrischer Kontakt  |a Plattieren  |a BorsÜÞure  |a Elektrolyt  |a Korrosionsschutz  |a Abriebfestigkeit  |a Zwischenschicht  |a Vernickeln  |a Palladium  |a Gold  |a Pilotanlagenma܃stab  |a Kontamination  |a Schmutzstoff  |a Arbeitssicherheit  |a KorrosionsbestÜÞndigkeit  |a Eigenspannung  |a Umweltschutz  |2 DE-601 
951 |a AR 
952 |d 95  |j 2017  |e 2  |h 73-77