Studies of silicon-containing bismaleimide resins - preparation and characteristics of reactive blends of silicon-containing bismaleimide and epoxy : Untersuchungen von Silikon-enthaltenden Bismaleinimidharzen - Herstellung und Charakterisierung von reaktiven Mischungen von Silikon-enthaltendem Bismaleinimid und Epoxid

Three kinds of silicon-containing bismaleimide (4,4'-Bismaleimido phenoxy silane) monomers were synthesized and added through blending to general epoxy system for the study of their applications as reactive flame retardants. The thermal analysis of the BMI monomers in bisphenol type epoxy system had... Full description

Contained in: International Polymer Processing Vol. 25, No. 2 (2010), p. 125-131
Fulltext access:
Availability is being checked...
Interlibrary loan: Check possibility for interlibrary loan
Links: Additional Link (dx.doi.org)
Additional Keywords: BISMALEINIMID
EPOXIDHARZ
FLAMMHEMMENDES-MITTEL
GLASUEBERGANGSTEMPERATUR
PYROLYSE
SAUERSTOFFMINIMALWERT
SILICON:POLYMER
WAERMEBESTAENDIGKEIT
ZERSETZUNGSTEMPERATUR
ZUGFESTIGKEIT
DOI: 10.3139/217.2303
Notes: Copyright: Metadaten: TEMA, Copyright WTI-Frankfurt eG
Copyright: (C) Alle Rechte beim Herausgeber
Physical Description: 7 Seiten, 7 Bilder, 3 Tabellen, 40 Quellen
ID (e.g. DOI, URN): 10.3139/217.2303
PPN (Catalogue-ID): WTI04858133X
Note: WTI TEMA DB
more publication details ...

Associated Publications/Volumes

  • Associated records are being queried...
more (+)
Internes Format
LEADER 02618nma a2200409 c 4500
001 WTI04858133X
003 DE-601
005 20190330121219.0
007 cr uuu---uuuuu
008 171222s2010 000 0 und d
024 7 |a 10.3139/217.2303  |2 doi 
028 5 2 |a TEMA2010_wti_pica 
035 |a (DE-599)WTI20100500630 
040 |b ger  |c GBVCP 
084 |a E  |2 FIZTtc 
084 |a 3KK  |a 3KXT  |a 3KXM  |2 FON2006 
245 0 0 |a Studies of silicon-containing bismaleimide resins - preparation and characteristics of reactive blends of silicon-containing bismaleimide and epoxy  |h Elektronische Ressource =  |b Untersuchungen von Silikon-enthaltenden Bismaleinimidharzen - Herstellung und Charakterisierung von reaktiven Mischungen von Silikon-enthaltendem Bismaleinimid und Epoxid 
300 |a Online-Ressource  |a 7 Seiten, 7 Bilder, 3 Tabellen, 40 Quellen 
500 |a Copyright: Metadaten: TEMA, Copyright WTI-Frankfurt eG 
500 |a Copyright: (C) Alle Rechte beim Herausgeber 
520 |a Three kinds of silicon-containing bismaleimide (4,4'-Bismaleimido phenoxy silane) monomers were synthesized and added through blending to general epoxy system for the study of their applications as reactive flame retardants. The thermal analysis of the BMI monomers in bisphenol type epoxy system had been discussed. An increase in the BMI contents decreased the storage modulus and glass-transition temperature and slightly reduced the mechanical strength of the epoxy blends. Although the initial pyrolysis temperatures of all the blending systems gradually decreased as the silicon-content increased, all the silicon-containing epoxy systems still had good thermal stability and the flame retardancy was promoted significantly by increasing contents of BML. The LOI values of all the blend types were increased to about 30 as the BMI concentration reached 20 %. 
653 4 |a BISMALEINIMID 
653 4 |a EPOXIDHARZ 
653 4 |a GLASUEBERGANGSTEMPERATUR 
653 4 |a ZERSETZUNGSTEMPERATUR 
653 4 |a SAUERSTOFFMINIMALWERT 
653 4 |a SILICON:POLYMER 
653 4 |a FLAMMHEMMENDES-MITTEL 
653 4 |a WAERMEBESTAENDIGKEIT 
653 4 |a ZUGFESTIGKEIT 
653 4 |a PYROLYSE 
773 0 8 |i In  |t International Polymer Processing  |g Vol. 25, No. 2 (2010), p. 125-131  |q 25:2<125-131 
856 4 0 |u http://dx.doi.org/10.3139/217.2303 
912 |a GBV_WTI 
950 |a Bismaleinimid  |a Epoxidharz  |a Glasübergangstemperatur  |a Zersetzungstemperatur  |a Sauerstoffminimalwert  |a Silikon (Polymer)  |a flammhemmendes Mittel  |a thermische Stabilität  |a Zugfestigkeit  |a Pyrolyse  |2 DE-601 
951 |a AR 
952 |d 25  |j 2010  |e 2  |h 125-131